Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.331 MPa | 48.0 psi | Cold Rolled Steel, 180°, after 48 hrs at 23°C |
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives 3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M |
|||
Shear Strength | 0.331 MPa | 48.0 psi | Galvanized Steel, 180°, after 48 hrs at 23°C |
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives 3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M |
|||
Shear Strength | 0.331 MPa | 48.0 psi | Stainless Steel, 180°, after 48 hrs at 23°C |
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives 3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M |
|||
Shear Strength | 0.331 MPa | 48.0 psi | Overlap, Polyethylene, 50% RH |
3M 5200 Marine Adhesive/Sealant 3M™ Marine Adhesive/Sealant 5200 is a one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds. It has excellent adhesion to wood, gelcoat and fiberglass. It for.. |