Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 1.52 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 1.52 MPa
220 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 1.52 MPa
>= 220 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-327 - 3/16 - 4.5 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Strength 1.52 MPa
220 psi
Plate Shear, W Direction
Hexcel® HexWeb® HRH-36 - 3/16 - 4.5 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Shear Strength >= 1.52 MPa
>= 220 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRP/F35 - 4.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength 1.52 MPa
220 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 1.52 MPa
220 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRH-10/F35 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength 1.52 MPa
220 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polycarbonate
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 1.52 MPa
220 psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polyacrylic
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 1.52 MPa

@Temperature 121 °C,
Time 900 sec
220 psi

@Temperature 250 °F,
Time 0.250 hour
Aluminum, Overlap
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 1.52 MPa
220 psi
Overlap, Neoprene Rubber/Steel; ASTM D1002
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Strength 1.52 MPa
220 psi
PE to PE
3M Scotch-Weld™ 3748 VO Hot Melt Adhesive
Self-extinguishing version of 3748 and Meets UL 1410 requirementsInformation provided by 3M