Mechanical Properties Metric English Comments
Shear Strength 1.81 MPa
262 psi
Overlap, Nylon
3M 5010 Polyurethane Multi-Purpose Adhesive
3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, f..
Shear Strength 1.81 MPa
262 psi
Overlap, ABS, 50% RH
3M 5200 Marine Adhesive/Sealant Fast Cure
A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals ..