Polymer Property : Shear Strength = 10.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 10.7 MPa

@Temperature 49.0 °C
1550 psi

@Temperature 120 °F
Overlap, Green FRP, AF/CF
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 10.7 MPa
1550 psi
Overlap, Gel Coat (3/16" thick), Substrate Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 10.7 MPa
1550 psi
Overlap, Steel, Adhesive Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..