Polymer Property : Shear Strength = 102 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength >= 0.700 MPa
>= 102 psi
ASTM C273
Parabeam Industrie Paraglass 5 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklay one-step process a lightweight and strong sandwich laminate is formed that offers excellent mechan..
Shear Strength 0.703 MPa
102 psi
Plate Shear, L Direction, typical value
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.0 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..
Shear Strength >= 0.700 MPa
>= 102 psi
ISO 1922
3A Composites Core Materials AIREX® T90.150 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Shear Strength >= 0.700 MPa
>= 102 psi
ISO 1922
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..
Shear Strength >= 0.700 MPa
>= 102 psi
ISO 1922
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Shear Strength >= 0.700 MPa
>= 102 psi
ISO 1922
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam
AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength..
Shear Strength >= 0.700 MPa
>= 102 psi
ASTM C273
Parabeam Industrie ParaTank 3 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..