Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 12.8 MPa | >= 1850 psi | Al/Al, Bond |
Master Bond EP21TDCN Two Component Nickel Conductive Epoxy Adhesive Product Description: Master Bond Polymer System EP21TDCN is a two component, nickel filled, electrically conductive, adhesive for high performance bonding, formulated to cure at room temperature or .. |
|||
Shear Strength | 12.8 MPa @Temperature 66.0 °C |
1850 psi @Temperature 151 °F |
Overlap, Oak, Substrate/Adhesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 12.8 MPa | 1850 psi | Overlap, Al/Al; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |