Mechanical Properties Metric English Comments
Shear Strength 876 MPa
127000 psi
Thickness not reported for this value
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Rod, 3 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter
Tensile strength (ultimate and yield), shear strength, reduction of area, and elongation values reported here are typical for Hot Finished Rod, 3 Part Heat Treatment, 0.562 inch (14.3 mm) Diameter s..