Mechanical Properties Metric English Comments
Shear Strength 9.31 MPa
1350 psi
Lap
Epoxy Technology EPO-TEK® H31D-LV Epoxy
Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i..
Shear Strength 9.31 MPa
1350 psi
3M Scotch-Weld™ DP605NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl..
Shear Strength 9.31 MPa
1350 psi
Overlap, Poplar, Substrate/Cohesive Failure
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 9.31 MPa
1350 psi
Overlap, Maple, Substrate Failure
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 9.31 MPa
1350 psi
Overlap, CRS/CRS after 7 days of Immersion in IPA
3M Scotch-Weld™ DP820 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..