Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 30.0 - 120 MPa | 4350 - 17400 psi | Average value: 74.6 MPa Grade Count:44 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Shear Strength | 100 - 120 MPa | 14500 - 17400 psi | 2mm/min.; IS 867-1963 |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |