Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 1.21 MPa | 176 psi | Overlap, Bronz, 50% RH |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |