Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 183 MPa | 26500 psi | Calculated |
Alcoa UltrAlloy® 6020-T8 Aluminum Weldability = B; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6020 characteristics and uses: Excellent machinability, high corrosion resi.. |