Polymer Property : Shear Strength = 19.48 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 19.3 - 19.48 MPa
2800 - 2825 psi
Tensile Shear Adhesion
3M Scotchkote™ FG 502 Epoxy Metal Repair
Scotchkote Epoxy Metal Repair FG 502 has been specifically developed as a 100% solids epoxy coating for resurfacing and reforming metal machinery and equipment. It also combines good application cha..
Shear Strength 19.3 - 19.48 MPa
2800 - 2825 psi
Tensile Shear Adhesion
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer
Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell..