Mechanical Properties Metric English Comments
Shear Strength 134 MPa
19500 psi
Punch test on film, unusually high for a polymer; ASTM D732
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..