Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.30 MPa | 334 psi | Typical; ASTM C273 |
Parabeam Industrie ParaTank 6 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Shear Strength | 2.30 MPa | 333 psi | Overlap, Glass |
3M 5010 Polyurethane Multi-Purpose Adhesive 3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, f.. |