Mechanical Properties Metric English Comments
Shear Strength 24.1 - 26.9 MPa
3500 - 3900 psi
ND Industries 388 Toughened Instant Superglue
Black toughened Cyanoacrylate for metal, rubber, and plastic
Shear Strength 24.1 - 26.9 MPa
3500 - 3900 psi
ND Industries Toughened Ethyl SuperGlue 310
Black flexible Cyanoacrylate for metal, rubber, and plastic