Mechanical Properties Metric English Comments
Shear Strength >= 18.0 MPa
>= 2610 psi
ASTM D1002/DIN 53283
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture...
Shear Strength 18.0 - 28.0 MPa
2610 - 4060 psi
Tensile, (Cured State)
Palm Labs Adhesives Turbo Fuse Series 115SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 115SI – SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture...
Shear Strength 18.0 - 28.0 MPa
2610 - 4060 psi
Tensile, (Cured State)
Palm Labs Adhesives Turbo Fuse Series 130SI Surface Insensitive (100 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th..
Shear Strength >= 18.0 MPa
>= 2610 psi
etched aluminum; ASTM D1002/DIN 53283
BCC Products BC 100 Medium Cyanoacrylate Adhesive
BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas..
Shear Strength 18.0 - 28.0 MPa
2610 - 4060 psi
tensile; ASTM D1002/DIN 53283
BCC Products BC 100 Medium Cyanoacrylate Adhesive
BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas..