Mechanical Properties Metric English Comments
Shear Strength 1.37895 - 29.6475 MPa

@Temperature -55.0 - 260 °C
200.000 - 4300.01 psi

@Temperature -67.0 - 500 °F
Average value: 17.4 MPa Grade Count:15
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
Shear Strength 1.37895 - 29.6475 MPa

@Time 0.000 - 4.41e+6 sec
200.000 - 4300.01 psi

@Time 0.000 - 1220 hour
Average value: 17.4 MPa Grade Count:15
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..