Polymer Property : Shear Strength = 3.05 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 3.05 MPa
443 psi
Valley Adhesives EM-221 Low Temperature Application Glue Stick
Valley Adhesives EM-221 Low Temperature Application Glue StickRapid strength build up to 0149; Excellent hot tack and wetting; Safe on styrofoam and heat sensitive materials; Bonds corrugated boxes ..