Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 3.79 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 3.79 MPa
550 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CFC™-20-1/8-9.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Shear Strength 3.79 MPa
550 psi
Plate Shear, W Direction, typ, preliminary
Hexcel® HexWeb® CR III 1/8-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 3.79 MPa
550 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 5/32-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 3.79 MPa
550 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 3.79 MPa
550 psi
Overlap, Polypropylene
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.Information provide..
Shear Strength 3.79 MPa

@Temperature 75.0 °C,
Time 1.81e+6 sec
549 psi

@Temperature 167 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre..
Shear Strength 3.79 MPa
550 psi
On Douglas Fir
3M Scotch-Weld™ 3796 Hot Melt Adhesive
High performance for plastics and light-gauge metalsInformation provided by 3M
Shear Strength 3.79 MPa
550 psi
Overlap, Acrylic
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b..
Shear Strength 3.79 MPa
550 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 3.79 MPa
550 psi
Overlap, PTFE, Adhesive Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 3.79 MPa
550 psi
Overlap, Gasoline for 14 days, Cohesive Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 3.79 MPa
550 psi
Overlap, Acrylic, Substrate Failure
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Shear Strength 3.79 MPa

@Temperature 32.0 °C
550 psi

@Temperature 89.6 °F
Overlap, Polyurethane Finish, 90% RH, Adhesive Failure
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 3.79 MPa
549 psi
Overlap, Oak, 50% RH
3M 5200 Marine Adhesive/Sealant
3M™ Marine Adhesive/Sealant 5200 is a one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds. It has excellent adhesion to wood, gelcoat and fiberglass. It for..
Shear Strength 3.79 MPa
550 psi
Overlap, HIPS, Substrate Failure
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 3.79 MPa

@Temperature 32.0 °C
550 psi

@Temperature 89.6 °F
Overlap, Polyurethane Finish, 90% RH, Adhesive Failure
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 3.79 MPa

@Temperature 75.0 °C,
Time 1.81e+6 sec
549 psi

@Temperature 167 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre..
Shear Strength 3.79 MPa
550 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, ABS PVC
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M