Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 32.0 MPa @Temperature 135 °C |
4640 psi @Temperature 275 °F |
0º, ILSS Short Beam, Wet; EN2563 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |
|||
Shear Strength | 32.0 - 45.0 MPa | 4640 - 6530 psi | IS 867-1963 |
Amity Thermosets ATS 132 Phenolic Molding Organic, inorganic, and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |