Polymer Property : Shear Strength = 365 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 2.52 MPa
365 psi
Plate Shear, L Direction
Hexcel® HexWeb® ACG®-1/4 Honeycomb Aluminum Commercial Grade
HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. ..