Polymer Property : Shear Strength = 3650 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 25.2 MPa

@Temperature 81.0 - 83.0 °C
3650 psi

@Temperature 178 - 181 °F
Etched Aluminum Overlap, 28.6% Ethylene Glycol/71.4% Tap Water Blend Immersion for 30 days
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M