Mechanical Properties Metric English Comments
Shear Strength 254 MPa
36800 psi
Calculated
Aleris Weldural Aluminum Alloy, 300 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..