Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 27.0 MPa @Temperature 150 °C |
3920 psi @Temperature 302 °F |
0º, ILSS Short Beam, Wet; EN2563 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |