Mechanical Properties Metric English Comments
Shear Strength 4.00 MPa
580 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP - 1/4 - 6.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 4.00 MPa
580 psi
Lap
Epoxy Technology EPO-TEK® M10-D Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
Shear Strength 4.00 MPa
580 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol Wipe surface prep, FRP
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M