Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 4.30922 - 24.4764 MPa @Temperature -55.0 - 391 °C |
625.001 - 3550.01 psi @Temperature -67.0 - 736 °F |
Average value: 11.9 MPa Grade Count:1 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |