Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.90 MPa | 421 psi | Typical; ASTM C273 |
Parabeam Industrie ParaTank 4.5 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |