Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 48.0 MPa | 6960 psi | ASTM D732 |
Unitika M1030B PA6, Conditioned Nano composite nylonInformation provided by Unitika Ltd. |
|||
Shear Strength | 48.0 MPa | 6960 psi | In-Plane |
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Shear Strength | 48.0 MPa @Temperature 71.0 °C |
6960 psi @Temperature 160 °F |
Compression interlaminar |
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric Information provided by HexCel |
|||
Shear Strength | 48.0 MPa | 6960 psi | 0º, ILSS Short Beam, RT, Dry; EN2563 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber Information provided by HexCel |
|||
Shear Strength | 48.0 MPa @Temperature 130 °C |
6960 psi @Temperature 266 °F |
In-Plane, Wet; EN6031 |
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 52%/G1177 Glass/Carbon Fiber Information provided by HexCel |