Shear Strength 50.3 MPa

@Temperature 149 °C
7300 psi

@Temperature 300 °F
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..