Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | >= 3.72 MPa | >= 540 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 5/32-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | >= 3.72 MPa | >= 540 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® HRP - 3/8 - 8.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Shear Strength | >= 3.72 MPa | >= 540 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR-PAA™ 3/16-5052-0.0025 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | >= 3.72 MPa | >= 540 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR-PAA™ 5/32-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 3.72 MPa | 540 psi | Overlap, Polycarbonate (IPA/abrade/IPA), Adhesive Failure; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | >= 3.72 MPa | >= 540 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 3/16-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |