Polymer Property : Shear Strength = 5530 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 38.1 MPa
5530 psi
Overlap, Aluminum Etched
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..
Shear Strength 38.1 MPa
5530 psi
Etched Aluminum Overlap, RT/50% RH for 14 days
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..