Polymer Property : Shear Strength = 563 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 3.88 MPa
563 psi
Valley Adhesives EM-110 High Performance Application Glue Stick
Valley Adhesives EM-110 High Performance Application Glue StickHigh peel, shear strength, and heat resistance; Good wetting and heat resistance for potting; Excellent adhesion to wood, plastics, pol..
Shear Strength 3.88 MPa
563 psi
Valley Adhesives EM-422 High Temperature Application Glue Stick
Valley Adhesives EM-422 High Temperature Application Glue StickRapid strength build up; Excellent hot tacking and wetting; Bonds corrugated boxes and paper in packaging operations and repackaging ar..