Mechanical Properties Metric English Comments
Shear Strength 6.07 MPa
880 psi
Overlap, Polycarbonate
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b..