Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 60.7 MPa @Temperature 21.1 °C |
8800 psi @Temperature 70.0 °F |
Short-Beam, Dry; Vacuum/Oven Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K 2x2 Twill Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 60.7 MPa @Temperature 23.0 °C |
8800 psi @Temperature 73.4 °F |
ASTM D732 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |