Mechanical Properties Metric English Comments
Shear Strength 0.460 MPa
66.7 psi
average; ISO 1922
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..