Polymer Property : Shear Strength = 72000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 496 MPa
72000 psi
Shear strength is 90% of tensile strength for all ductile iron grades
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for..
Shear Strength 496 MPa
72000 psi
Shear strength is 90% of tensile strength for all ductile iron grades
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for..