Mechanical Properties
Metric
English
Comments
Shear Strength
51.97
MPa
7538
psi
ASTM D732
Network Polymers Kepital® TC30-20
Description: Natural Acetal Copolymer, 10% Talc Reinforced GradeInformation provided by Network Polymers Inc.