Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 7600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 52.4 MPa

@Temperature 23.9 °C
7600 psi

@Temperature 75.0 °F
Short-Beam, Dry; Oven Cure 275°F, 90 min; ASTM D2344
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Shear Strength 52.4 MPa
7600 psi
ASTM D732
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet)
Shear Strength 52.4 MPa
7600 psi
Ultimate; ASTM D3846
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex..
Shear Strength 52.4 MPa

@Temperature 22.8 °C
7600 psi

@Temperature 73.0 °F
Ultimate; ASTM D3846
Ensinger Tecapeek® Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
Shear Strength 52.4 - 62.1 MPa
7600 - 9000 psi
ASTM D732
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon
Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau..
Copyright © lookpolymers.com All Rights Reserved