Shear Strength 5.50 MPa
798 psi
ASTM C273
3A Composites Core Materials AIREX® PXc.420 Fiber-Reinforced Structural Foam
AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu..