Polymer Property : Shear Strength = 8.446 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 8.446 MPa
1225 psi
Overlap, Oily HDG, Adhesive/Cohesive Failure
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Shear Strength 8.446 MPa
1225 psi
Overlap, PE, Substrate Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..
Shear Strength 8.446 MPa
1225 psi
Overlap, ED-5000 E-Coated CRS/HDPE, Adhesive Failure
3M Scotch-Weld™ DP8010 Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl..