Mechanical Properties Metric English Comments
Shear Strength 41.0 - 57.0 MPa
5950 - 8270 psi
Average value: 49.0 MPa Grade Count:4
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..