Shear Strength 85.0 MPa
12300 psi
ASTM D732
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, at 50% RH &n
AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage..
Shear Strength 85.0 MPa
12300 psi
0°, Short Beam
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape Not Supported 150 g/m2
Information provided by HexCel
Shear Strength 85.0 - 95.0 MPa
12300 - 13800 psi
IS 867-1963
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..