Mechanical Properties Metric English Comments
Shear Strength 597 MPa

@Strain 0.200 %,
Thickness 19.0 - 31.8 mm
86600 psi

@Strain 0.200 %,
Thickness 0.750 - 1.25 in
Crucible Steel Aquamet® 22 Stainless Steel
AQUAMET 22 is a high-alloy stainless steel with superior corrosion resistance along with excellent toughness and high strength. It has higher strength than AQUAMET 17 in 3/4" to 1-1/4" dia., and it ..