Polymer Property : Shear Strength = 88.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.607 MPa
88.0 psi
Overlap, Polyacrylic
3M Scotch-Weld™ DP405 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..