Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 66.9 MPa | 9700 psi | ASTM D732 |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Shear Strength | 66.9 MPa | 9700 psi | ASTM D732 |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |