Polymer Property : Shear Strength = 9900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 68.3 MPa

@Temperature 65.6 °C
9900 psi

@Temperature 150 °F
Greene Tweed Arlon® 1330 PEEK
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
Shear Strength 68.3 MPa

@Temperature 65.6 °C
9900 psi

@Temperature 150 °F
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..