Polymer Property : Secant Modulus, MD = 0.107 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.107 GPa
15.5 ksi
ASTM D882
Huntsman PE1605 EVA Film Extrusion  (discontinued **)
6% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi..