Polymer Property : Secant Modulus, MD = 0.108 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.108 GPa
15.7 ksi
5%; ASTM D882
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend
The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film..
Secant Modulus, MD 0.108 GPa
15.7 ksi
2% Secant; ASTM D882
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g..