Polymer Property : Secant Modulus, MD = 0.1806 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.1806 GPa
26.20 ksi
2% Secant; ASTM D882
Dow DOWLEX™ 2078G Linear Low Density Polyethylene
Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow