Mechanical Properties Metric English Comments
Secant Modulus, MD 0.186 GPa
27.0 ksi
0.01; ASTM D882
Eastman 1925F Polyethylene Film  (discontinued **)
Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good..
Secant Modulus, MD 0.186 GPa
27.0 ksi
1% Secant; ASTM D882
Eastman E6838-795F Polyethylene  (discontinued **)
E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag..
Secant Modulus, MD 0.186 GPa
27.0 ksi
1% Secant; ASTM D882
Eastman E6838-796F Polyethylene  (discontinued **)
E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen..
Secant Modulus, MD 0.186 GPa
27.0 ksi
0.01; ASTM D882
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services  (discontinued **)
Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced..
Secant Modulus, MD 0.186 GPa
27.0 ksi
1% Secant; ASTM D882
Eastman D4036-F Polyethylene  (discontinued **)
D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener..
Secant Modulus, MD 0.186 GPa
27.0 ksi
1% Secant; ASTM D882
Eastman E6838-963F Polyethylene  (discontinued **)
E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati..
Secant Modulus, MD 0.186 GPa
27.0 ksi
ASTM D882
Huntsman PE8010 Specialty Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1..